SSPC-Paint 27


SSPC-Paint 27

Specifications


Asset:  Onshore Structure
Environmental Characteristic:  Below Freezing Point, High Humidity, Low Humidity
Industry:  Misc. Corrosion
Process:  Application
Substrate:  Carbon Steel, Aluminum, Misc. Alloys

Summary


Basic Zinc Chromate-Vinyl Butyral Wash Primer

Description


This specification covers a two-component basic zinc chromate-vinyl butyral wash primer for structural steel surfaces prior to painting. \r\nIt is intended that this coating be used primarily on clean steel free of rust and scale or on clean galvanized metal cleaned according to SSPC-SP 1, Solvent Cleaning; but it may be used, when specified, on steel with very slight amounts of rust. It is to be applied by brush or spray in accordance with SSPC-PA 1, Shop, Field, and Maintenance Painting of Steel.