The Science of Anti-Corrosion Thin Films

By Sadeq Hooshmand Zaferai, MSc
Published: March 12, 2020
Key Takeaways

Since the early 1900s, thin films have been explored for corrosion protection of metals. Through many decades of development, the thin films of today offer a range of unique characteristics for many types of industry applications.

Source: S. H. Zaferani

Nanocoatings are defined as the nanostructures with thickness in the nanometer scale. Generally, thin film builds are required to have a thickness in a range of a micron or less with special characteristics in production, performance, and application.1

Advertisement

The history of the thin films goes back more than a century, progressing over many decades. For example, the first deposition of diamond-like polycrystalline carbon was achieved in 1911, and active research and development of amorphous carbon (a-C) thin films was performed in the 1970’s.2 Many more types have been formulated since with varying degrees of success. (Learn more about The Composition of a Paint Coating.)

Various thin film coating chemistries and a full range of application techniques yield unique performance characteristics, such as anti-corrosion, self-cleaning, and chemical resistance and scratch resistance.3 Figure 1 summarizes a variety of ways in which thin films can be produced and applied.

Advertisement

Figure 1. Application techniques of thin films4

Figure 1. Application techniques of thin films.

The development of effective anti-corrosion pre-treatments for metallic substrates has attracted a lot of attention, owing to their ability to increase the durability of metal structures and components in aggressive environments (e.g., aqueous, NaCl, HF, HCl, alkaline media).

Advertisement

Regulatory Hurdles

When first introduced, conventional chromate conversion coatings (CCC) were considered good candidates based on their corrosion protection performance. The self-healing nature of CCCs, ease of application and high electric conductivity contributed to the early adoption of chromate coatings by the industry. (Learn more in the article A Look at Self-Healing Metal Oxides as a Corrosion Prevention Method.)

However, the strong oxidation characteristics of chromates were shown to cause human DNA damage and a heightened risk of lung cancer with exposure. Consequently, the demand for more environmentally friendly coatings increased due to strict environmental legislation and tightened regulations on the use of hexavalent chromate. (Discover how to Write Safety Into Your Coating Specification.)

Advertisement

Development of Safer Alternatives

In the late 1990s, chromate-free thin films were introduced as a safer choice to enhance the corrosion resistance of metallic components. In formulating these coatings, more attention has been paid to the statistical design and functionality of polymers to ensure better uniformity of crosslinking during curing, and to ameliorate film performance.

Among the new techniques for thin film production, sol-gel was evaluated positively for adhesion to both metallic substrates and organic top coats for use as an intermediate. Economically viable production is a crucial factor in choosing sol–gel coatings for anti-corrosion protection.

Incorporation of nanoparticles in hybrid sol–gel systems improve corrosion protection properties as a result of lower porosity, increased thickness and diminished cracking potential along with enhanced mechanical properties.4,5 The concentration of nanoparticles is a vital factor in the final performance characteristics.

One way to produce thin films with self-repairing and anti-corrosive properties is to add healant components, such as corrosion inhibitors and rare earth elements. By controlling the release rate of these healant components, the durability of the coating can be managed.6

Moreover, self-assembling molecules provide valuable coating performance on the basis of their close and regular arrangement on the metal surface, and polymerize afterwards. Hence, this ability provides an extremely flexible, strongly anchored layer for improving coating adhesion, corrosion protection, and mechanical and chemical resistance.7

In this field, silane-based thin films are another promising type that can provide a wide range of useful characteristics.8 Silane films formed from silane monomers in a solution are environmentally friendly types that were evaluated in several studies.9

Silane-based thin films are represented as the following structure:8

  1. R (CH2)n Si X3 (1) [Where R donates organo-functional groups, X3 is a hydrolysable group and (CH2) n alkyl chain acts as linker]
  2. R-Si-OR’+H2O ?R-Si-OH+R’-OH
  3. 2R-Si-OH?R-Si-O-Si-R+H2O
  4. M-OH+R-Si-OH?M-O-Si-R+H2O

In equations 2 through 4, the notations R and R’ are functional methyl or ethyl group respectively. M stands for metal. Equations 2 to 4 show the hydrolysis and condensation of silane films, depicted in Figures 2 and 3 below.

Figure 2. Structure of silane films in different stages after application8

Figure 2. Structure of silane films in different stages after application.

Figure 3. Bonding of silane coupling agents to mineral surface8

Figure 3. Bonding of silane coupling agents to mineral surface.

The final thin film can exhibit desirable adhesion to the metal substrate due to the formation of chemically adsorbed M–O–Si bonds to the top-coated organic coatings by properly choosing the R group. The resultant film also provides good corrosion performance because of the formation of highly dense – [Si–O–Si] – bone structure on the basis of the selected R group.

To sum it up, corrosion is a major factor that can diminish the efficiency of the metallic component performance in several fields. This critical issue presents large-scale industrial concerns in energy-providing infrastructures and transportation systems, and is commonly discussed to ensure continuous operation and maintain the desirable efficiency.

Various techniques have been explored to control, manage and mitigate the corrosion phenomena, and anti-corrosion films have received a lot of attention. There are wide applications of protecting films; for example in marine conditions, anti-corrosive films for splash zones, risers and abrasion-resistance above or below water, encapsulated compounds (dopant with healant) films, UV protection films, etc., are some subjects that are prevalent among the marine structure maintenance. (For a deep dive, see Coatings for Marine Applications and Offshore Platforms.)

Several experiments have been designed to prove the ability of metallic structures to withstand years of exposure in harsh environments:

Through these methods, thin films are specifically engineered for optimum corrosion protection, as well as to maximize coating adhesion, generate excellent impact resistance, and improve abrasion, flexibility and slip resistance in the most challenging conditions.

In a wide range of research over many decades, enhancing the protection of iron and steel has been evaluated by applying the effective anti-corrosive, non-chromate and low-VOC films. In this field, silane-based thin films are candidates due to their exceptional ability to form strong bonds to metal substrates and, at the same time, to form cross-linking polymers on the surface, both of which contribute to producing strong conversion coatings.

***

References

  1. K. L. Mittal, Adhesion measurement of thin films, Electrocomponent Science and Technology 1976, Vol. 3, pp. 21-42.
  2. W.B. Nowak, Thin metallic films for corrosion control, Surface and Coatings Technology. 49 (1991) 71—77.
  3. A. M. Hofer, G. Mori, A. Fian, J. Winkler, C. Mitterer, Improvement of oxidation and corrosion resistance of Mo thin films by alloying with Ta, Thin Solid Films 599 (2016)
  4. A. S. Hamdy Makhlouf, I. Tiginyanu, Nanocoatings and ultra-thin films, Woodhead Publishing Limited, ISBN 978-0-85709-490-2, 2011.
  5. M. Abuín, A. Serrano, J. Llopis, M.A. García, N. Carmona, Silica doped with lanthanum sol–gel thin films for corrosion protection, Thin Solid Films 520 (2012) 5267–5271.
  6. S. Hooshmand Zaferan, M. Peikari, D. Zaarei, I. Danaei, J. Mostowfi Fakhraei, Self-healing property of cerium nitrate in organosilane pretreated coatings, SPE International Conference and Exhibition on Oilfield Corrosion held in Aberdeen, UK, 28–29 May (2012), ISBN: 978-1-62276-080-0.
  7. D. Wang, Y. Ni, Q. Huo, D.E. Tallman, Self-assembled monolayer and multilayer thin films on aluminum 2024-T3 substrates and their corrosion resistance study, Thin Solid Films 471 (2005) 177– 185.
  8. S. Hooshmand Zaferani, M. Peikari, I. Danaee, D. Zaarei, J. Mostowfi, Fakhraei, M. Mohammadi, Using Silane Films to Produce an Alternative for Chromate Conversion Coatings, Journal of Corrosion, NACE, Houston, Vol. 69, No. 4, April (2013), 372-387.
  9. S. Hooshmand Zaferani, I. Danaee, Investigating the Effect of Organosilane and Cerium Nitrate on High- performance Epoxy-based Coatings for Carbon Steel, ISBN-13:978-3-659-44715-0, ISBN- 10:3659447153,EAN: 9783659447150, LAP LAMBERT Academic Publishing, 2013.

Share This Article

  • Facebook
  • LinkedIn
  • Twitter
Advertisement
Sadeq Hooshmand Zaferai, MSc
Corrosion Engineer, POGC, NIOC

S. H. Zaferai currently works as Senior Technical Inspector and Corrosion Engineer for Pars Oil and Gas Company (POGC), National Iranian Oil Company (NIOC), and also serves on the editorial board of the Journal of Adhesion Science and Technology.

In articles and technical papers published by NACE, Taylor and Francis, Elsevier and SPE, Zaferai has explored technical inspection techniques, failure mechanisms, failure analysis, corrosion and protective coatings and nondestructive testing, with a focus on environmental challenges in the oil and gas and renewable energy industries.