SSPC-PS 11.01


SSPC-PS 11.01

Specifications


Asset:  Offshore Structure, Onshore Structure, Pipeline
Environmental Characteristic:  Below Ground, Fresh Water, High Humidity, Low Humidity
Industry:  Pipelines and Underground Systems, Water and Wastewater, Transportation Infrastructure, Maritime
Process:  Application
Substrate:  Carbon Steel

Summary


Black (or Dark Red) Coal Tar Epoxy Polyamide Painting System

Description


This specification covers a complete coal tar epoxy polyamide black (or dark red) painting system for the protection of steel surfaces that will be exposed to severely corrosive conditions.\r\n\r\n\r\n\r\nThis system is suitable for use on parts or structures exposed in Environmental Zones 2A (frequently wet by fresh water), 2B (frequently wet by salt water), 2C (fresh water immersion), 2D (salt water immersion), 3A (chemical, acidic), 3B (chemical, neutral), and 3C (chemical, alkaline). Its resistance to chemical fumes, mists, and splashings is generally considered to be good, but its suitability for prolonged immersion in specific chemicals should be confirmed by trial tests in the absence of applicable case histories. It is also suitable for underground exposure and as a protective coating for sound concrete surfaces in marine and some chemical environments.