Rust staining refers to the occurrence of a paint defect that is due to the discoloration of an applied coating on a substrate. The discoloration occurs due to the accumulation of reddish colored iron oxide deposits. Such paints are applied to metal surfaces as protection against corrosion. View Full Term
Trending Terms
Corrosionpedia Terms
Connect with us
Subscribe To Our Newsletter
By clicking sign up, you agree to receive emails from Corrosionpedia and agree to our Terms of Use and Privacy Policy.
Free Webinar: Flange Isolation and Remote Monitoring
An Innovative Coating Solution for Oil Sands Equipment Using a Chromium Carbide Weld Overlays
By: Jessica Zimmer
Polyurea coatings are preferred where other coatings fail to protect the substrate. They have the unique advantage of moisture resistance, rapid curing, and...
By: Shivananda Prabhu
Pitting corrosion can have serious implications because the cavity it bores below the surface can be both wide and deep, thus seriously affecting the load...
Polyurea is commonly used as a waterproofing sealant and corrosion-resistant coating on metals and concrete surfaces. The reasons for its...
Due to the potential for soluble salts to reduce coating performance, testing the substrate for the presence of these salts should be considered a requirement
By: Heather Stiner | Protective Coatings Professional, SSPC
Jane Debbrecht discusses the electroplating process, how it is used in industry, and the benefits it has over other corrosion prevention techniques.
By: Corrosionpedia Staff
Sanitation corrosion is a worldwide problem that permeates through a system of moving waste to processing stations, often ending with water reclamation. As the
By: Robert Anderson
Corrosive deterioration of the critical surfaces of aircraft can come in the way of ensuring a reliable and safe operational performance. If the corrosion is n
The 5 most common types of metal coatings that can effectively prolong the service life of many metal assets by preventing corrosion...
By: Krystal Nanan | Civil Engineer
Ian MacMoy, an expert on pressure bolt coatings for aggressive corrosion environments, speaks out against oversizing nut threads to accommodate thick bolt coatings, a common practice banned by the standards for bolts that secure high pressure and load.
By: Alan Kehr | Managing Consultant, Alan Kehr Anti-Corrosion, LLC
Quality assurance specialists are usually employed or subcontracted by an asset owner. In the paint and coatings industry, they verify that the work performed by the quality control team meets the documented minimum job specifications.
Metallizing is a general term used to describe the process of applying a metallic coating on the surface of an object. It involves several processes that cause the coating metal to form a mechanical bond with the substrate.