Key Takeaways

Corrosion in process vessels and tanks is problematic; here are some protection system options that take into account the total cost of ownership of these assets.

Source: Pichit Boonhuad/Dreamstime.com

When selecting a suitable protection system for process vessels and tanks, we need to not only look at the cost of a unit, but the total expenditure. This can include coverage rate, length of downtime and costs of application based on its simplicity or difficulty among others. The list goes on, and ultimately a system that is cheaper to procure may turn out to be more expensive after the total expenses are tallied. In this article, we review how selection and maintenance of a corrosion protection system can contribute toward the operating expenditure.

Advertisement

We will look at more aggressive environments of elevated temperature immersion service with relatively corrosive acids or alkalis and some degree of erosion or abrasion. These processes can be common in piping and process vessels in the oil and gas upstream and downstream sectors as well as petrochemical, chemical and mineral processing industries. Here, chemicals such as sulfuric acid and hydrochloric acid in combination with sea water and erosive slurries can quickly eat away at the base metal, typically carbon steel.

The industry has moved away from high corrosion allowances of the base metal to applying corrosion protection, which is able to extend the lifetime of the asset to an average of 20 to 30 years.

Advertisement

Material selection for protecting the base metal can include a variety of options – exotic alloys, metallic cladding, and epoxy and rubber linings, among others. Exotic alloys and metallic cladding understandably have very high capital expenditures, whereas the rubber lining option would be on the opposite side of the spectrum. A rubber lining is relatively cheap, but due to its permeability and swelling potential, it is not the most reliable corrosion protection solution against harsh chemicals. (For more ideas, read Choosing a Fit-for-Service Lining System for Process Vessels.)

We will focus on alternative options that seem to sit in between, and highlight their advantages as well as the risks potentially associated with their use, giving some recommendation when each would be more suitable.

Advertisement

Glass Linings

Glass-lined steel provides superior corrosion resistance to acids, alkalis, water and other chemical solutions (with the exception of hydrofluoric acid and hot concentrated phosphoric acid). As a result of this chemical resistance, a glass lining can serve for many years in environments that would quickly render most metal vessels unserviceable.

At higher temperatures, glass is not as effective against alkalis, where an increase by 18ºF (10ºC) doubles the rate of attack on glass. Glass performs well in a variety of operating conditions, offering excellent resistance to corrosion. Its anti-adhesive properties make it very suitable for use in the chemical and pharmaceutical industries.

Advertisement

Of course, as a glass lining provides protection against extremely aggressive environments, its costs are directly proportional. In addition, glass linings are very susceptible to impact damage and the subsequent repairs can be very costly. For milder service conditions, a glass flake technology can be considered.

Coatings Containing Glass Flakes

Glass flakes have been used to improve both barrier properties and reinforcement in anti-corrosion coatings since the early 1970s. Nowadays, glass flake based coatings are used in a variety of industrial sectors due to their good chemical and erosion resistance.

There is a relatively poor understanding of how the glass bonds within the various resin matrices, and although glass flake coatings are impervious to moisture vapor and gas diffusion, it does not present a continuous barrier in a resin matrix. The resin carrier, therefore, plays a very important role, i.e., glass flake cannot make a poor resin film into an excellent coating, although it may substantially improve it.

Vinyl ester is one of the more common resins used with glass flakes, which offers benefits in terms of cost savings, but also has several drawbacks. The polymerization involved in the curing process of the glass flake system leads to shrinkage, causing the bond line to be permanently stressed. Adhesion is also found to be inferior to that of an epoxy-based system. The system can also be brittle and easily damaged during inspection or maintenance. The cure mechanism, inhibited by atmospheric oxygen, can lead to significant coating voids that will lead to failure, particularly in decompression situations, which was confirmed by a test sponsored by a global group of energy and petrochemical companies.

Vinyl ester glass flake systems can therefore be quite suitable for pipeline protection or storage tanks, but not ideal for use in pressurized equipment.

Organic Epoxy Coatings

Epoxy coatings, such as ceramic-filled, modified epoxy novolac or high molecular weight polymer composites have been on the market for many years and are continuously “modified” with the use of new raw materials to improve their features, including temperature resistance, abrasion resistance, adhesion and sprayability for ease of application.

Ceramic-filled epoxies are widely used for erosion corrosion protection, with the first application on a process vessel carried out in 1987 when a separator was protected at a North Sea platform in the U.K. Their limitation comes in the form of temperature resistance and sprayability, with both of these issues later addressed by the introduction of modified epoxy novolac, which are able to continuously resist immersion temperatures up to 320ºF (160ºC) and high molecular weight polymers, which offer superior erosion resistance while being “spray-friendly”.

There are some risks associated with the use of epoxy coatings, which mainly presented in the form of applicator error and incorrect coating specification. Both can be addressed with appropriate training and guidance provided by the material manufacturer.

Where epoxy coatings are limited in terms of temperature and chemical resistance, polytetrafluoroethylene-based coatings can be used.

Polytetrafluoroethylene (PTFE) Coatings

Polytetrafluoroethylene (PTFE) coatings are commonly used in situations where superior corrosion resistance is required. Fluoropolymers are the materials of choice for the process industry, serving as linings for vessels, piping, pumps, valves, columns, column internals, hoses, expansion joints, seals and gaskets. They provide durable low maintenance alternatives to exotic metal alloys, offering thermal stability for use at high temperatures. In addition, because they do not react with the process liquids, they prevent contamination.

PTFE is electrochemically, biochemically, enzymatically and chemically virtually inert. Just as important, the useful properties are retained at up to 392ºF (200ºC), giving PTFE the highest retention of its chemical properties of any known plastic-like material (i.e., not more than 15% loss of chemical resistance).

Unfortunately, PTFE comes with a number of unhelpful properties when used to move corrosive materials around. It is necessary to understand these in order to manage them. Because of a lack of intermolecular forces, the material is soft and easily abraded. This means that erosion is a potential concern, as is the property of creep or cold flow under load. PTFE is also difficult to repair if damaged, as this cannot be done in situ.

Case Study of Selecting an Appropriate Barrier Coating

An example case study may be enlightening:

A polyolefins petrochemical plant based in Ferrara, Italy, was looking for a new coating system for their reactor, which was operating between 158ºF (70ºC) and 176ºF (80ºC) and processing salt, caustic and titanium tetrachloride. The original hot-applied PTFE lining required maintenance due to localized disbondment, which was caused by minor abrasion of the titanium compound. As a result, the plant was facing a long downtime (between two and four weeks) as it was not possible to conduct an in-situ repair.

The maintenance manager was keen to keep the downtime to an absolute minimum and ultimately decided to replace the PTFE with a 100% solids modified epoxy novolac system, Belzona 1593, designed for elevated temperature immersion up to 320ºF (160ºC). Belzona 1593 was hand applied onto the reactor in April 2015, facilitating its return to service within only four days.

Belzona 1593 was hand applied onto the reactor in April 2015, facilitating its return to service within only four days.

An added benefit, which was considered during material selection, was the servicing of the lining. As this system is applied at ambient temperatures and adheres well to metal and to itself, it can be repaired in situ when necessary. A similar epoxy system, for instance, has now remained in service on a test separator at a North Sea platform for 20 years, being patch repaired once every decade during regular inspections.

The reactor was opened for inspection in September 2015 and the maintenance manager was very satisfied with the result. If the lining were to start failing due to poor chemical resistance, this first inspection would have revealed visible signs of degradation. As the lining was found to be fully intact, its durability was not questioned. Moreover, they were able to save time by steam cleaning the reactor, which was not previously possible with the PTFE lining. They are now looking at replacing the lining on other existing reactors as well as protecting new reactors with the same 100% solids modified epoxy novolac system.

Savings resulting from reduced downtime along with simplified cleaning and maintenance protocols in this case significantly outweighed the initial cost of material.

Share This Article

  • Facebook
  • LinkedIn
  • Twitter
Advertisement

Presented By

Logo for Belzona Inc.
Corrosionpedia Staff

Corrosionpedia aims to provide the first steps in the research journey for asset integrity professionals the world over.

Working with our team of internal writers, contractors and third-party experts, we source world leading educational content on the subject of preserving the long-term integrity of the world's infrastructure and assets. We designed our proprietary platform to fit the needs of the industry, and build the in-demand tools to help connect industry professionals to the solutions and solutions providers they need.

Related Articles

Go back to top