What Does Sling Psychrometer Mean?

A sling psychrometer is a hygrometer that can be rotated in the air to make a wet-bulb attain a constant value. It is used to determine the atmospheric humidity in a given area.

Advertisement

Corrosionpedia Explains Sling Psychrometer

A sling psychrometer is used to determine the atmospheric humidity of an environment that surrounds a given metal application.

High moisture levels in the immediate vicinity of a metal can contribute to higher corrosion rates due to the formation of aqueous ions. The use of a sling psychrometer facilitates the proper corrosion prevention methods to be taken in a timely manner depending on the observed moisture levels.

Advertisement

Share This Term

  • Facebook
  • LinkedIn
  • Twitter

Related Reading

Trending Articles

Go back to top

Stay Ahead of the Corrosion Curve

Get expert insights, industry news, and practical tips delivered straight to your inbox. Join our community of corrosion professionals.