Question

How can I determine what blast pressure is best for my application?

Answer
By Wade Hannon | Published: May 31, 2018 | Last updated: August 5, 2020
Presented by Graco Inc.

The blast pressure directly determines the velocity of the blast media through the blasting nozzle, and therefore the impact force on the substrate.

While there are a wide range of pressures that can accomplish the same job, choosing the optimal pressure for a specific application requires balance. Blast pressures that are set too low can drastically reduce the speed and efficiency of blast cleaning. On the other hand, pressures that are too high can shatter the abrasive media upon impact, resulting in reduced energy transfer and cleaning efficiency.

One of the most significant factors that determine the optimum blast pressure for a specific application is the type of material that needs to be removed. Lower pressures are adequate for the removal of thin coatings, dirt and grease, while higher blast pressures are necessary to remove sturdier materials such as rust and heavy coatings. Higher pressures may also be required to clean small and hard to reach areas.

Another factor to take into consideration is the profile depth or surface preparation standard that needs to be achieved (e.g., white metal, near white metal, etc.). For example, in instances where coatings or contaminants require removal without changing the surface profile of the substrate, excessively high pressures may not be appropriate. (Discover the 6 Ways to Measure Surface Profiles for Concrete Surface Preparation.) It is therefore essential that the required profile and the substrate material be analyzed beforehand to determine the most appropriate blast pressure.

Finally, the material to be cleaned must also be taken into consideration. Abrasive blast cleaning can potentially damage the substrate if the pressure is set too high. Wood, for example, needs to be cleaned at relatively lower pressures (when compared to steel) to avoid damage to the wood fibers.

The table below gives some ballpark values for appropriate blast pressures for various materials and situations. It is only intended to be used as a guide; fine-tuning of the blast pressure in the field is recommended to ensure the desired results are achieved.

table of blast pressures for various materials and applications

Advertisement

Presented By

Logo for Graco Inc.

Share this

  • Facebook
  • LinkedIn
  • Twitter

Written by Wade Hannon | Area Sales Manager, Specialty Products at GRACO Inc.

Wade Hannon
Wade Hannon is an Area Sales Manager – Specialty Products at GRACO Inc. with responsibilities for equipment demonstrations, technical support, distributor development and sales support, marketing and promotion within assigned territories, trade shows and internal sales support.

More Q&As from our experts

Term of the Day

Rust Staining

Rust staining refers to the occurrence of a paint defect that is due to the discoloration of an applied coating on a…
Read Full Term

Don't miss the latest corrosion content from Corrosionpedia!

Subscribe to our newsletter to get expert advice and top insights on corrosion science, mitigation and prevention. We create world-leading educational content about corrosion and how to preserve the integrity of the world’s infrastructure and assets.

Resources
Go back to top