What Does Bleeding Mean?

Bleeding is a kind of paint defect. Bleeding refers to the diffusion or seeping of a soluble dye from the substrate through the top coat color. In general, bleeding causes a spot-like discoloration of the top coat, mostly producing a reddish or yellowish color. In bleeding, the undercoat stains through the top coat, so bleeding could be a source of corrosion of the substrate.

To prevent coating failure, it is important to use dye stuffs with sufficient solvent resistance to prevent bleeding.


Free Coating Failures and Defects Guide – Sponsored by Fitz’s Atlas 2

Coating Failures and Defects Guide
Click here to download your free guide!


Advertisement

Corrosionpedia Explains Bleeding

Bleeding is a coating defect causing unwanted discoloration on the upper coat. This is caused by the diffusion of pigments and/or dye stuffs from the lower coat of coating film to the upper coat from an excessive use of solvents (sometimes resins). Bleeding often appears where bituminous or tar-based products are overcoated with top coats. Tar or bitumen are solubles in top coats and cause this bleeding. Bleeding is also seen with emulsion paints.

Causes of bleeding:

  • Use of excessive peroxide with the putty
  • Inadequate mixing of the hardener with the putty
  • Lack of isolation-sensitive colors
  • Improper surface cleaning
  • Soluble dyes from the old paintwork are dissolved in the solvent of the repair materials, and change in the shade at the surface
  • Residues from bitumen and tar

To avoid paint bleeding, use the correct coating specification, appropriate sealer coat and compatible materials; and remove all contamination including bitumen and tar deposits before painting.

The paint bleeding area can be repaired by removing the stained or contaminated layer and applying a suitable sealer coat to prevent the diffusion of soluble-colored material from the substrate. Apply a sealer coat to remove the stained or contaminated layer.

Advertisement

Share This Term

  • Facebook
  • LinkedIn
  • Twitter

Related Reading

Trending Articles

Go back to top