The Use of Laser Scanning when Conducting Fitness-for-Service Corrosion Assessments The Use of Laser Scanning when Conducting Fitness-for-Service Corrosion Assessments The Use of Laser Scanning when Conducting Fitness-for-Service Corrosion Assessments The Use of Laser Scanning when Conducting Fitness-for-Service Corrosion Assessments


Laser scanning (profilometry) is a highly effective and accurate inspection method for measuring changes in geometry of pressurized vessels...

Strategy for a Corrosion Remediation Program Strategy for a Corrosion Remediation Program Strategy for a Corrosion Remediation Program Strategy for a Corrosion Remediation Program


A quick overview of the recommended steps in order to establish a robust corrosion remediation program that delivers a quality result and...

Use of Non-intrusive Inspection in Onshore Gas Facilities Use of Non-intrusive Inspection in Onshore Gas Facilities Use of Non-intrusive Inspection in Onshore Gas Facilities Use of Non-intrusive Inspection in Onshore Gas Facilities


Non-intrusive inspections of pressure and process vessels are used to determine the internal condition of the equipment without having to...

Lessons Learned from 50 Years of Coatings Testing at SA Water Lessons Learned from 50 Years of Coatings Testing at SA Water Lessons Learned from 50 Years of Coatings Testing at SA Water Lessons Learned from 50 Years of Coatings Testing at SA Water


This article provides key findings and lessons learned from test results generated across eight environmental test sites with the aim of...

Protecting Pipelines from Corrosion Under Insulation Protecting Pipelines from Corrosion Under Insulation Protecting Pipelines from Corrosion Under Insulation Protecting Pipelines from Corrosion Under Insulation


Corrosion under insulation (CUI) prevention with thermal sprayed aluminum (TSA) provides long-term and reliable prevention that reduces...

What Does Quality Control Mean in the Corrosion and Coatings Industry? What Does Quality Control Mean in the Corrosion and Coatings Industry? What Does Quality Control Mean in the Corrosion and Coatings Industry? What Does Quality Control Mean in the Corrosion and Coatings Industry?


Quality control on a job site is often standardized by regulatory agencies in a way that makes it completely objective, and hence...

How Hot Shortness and Welding Affect Corrosion in Metals How Hot Shortness and Welding Affect Corrosion in Metals How Hot Shortness and Welding Affect Corrosion in Metals How Hot Shortness and Welding Affect Corrosion in Metals


Hot shortness is a welding defect that can cause cracking of the metal surface as it cools. These cracks can serve as breeding grounds for...

Installation Methodology for Compliant Composite Repairs Installation Methodology for Compliant Composite Repairs Installation Methodology for Compliant Composite Repairs Installation Methodology for Compliant Composite Repairs


The proper installation of composite repairs to corroded piping or equipment requires special training and application methods.

Understanding a New Trend: In Situ Cleaning and Coating Understanding a New Trend: In Situ Cleaning and Coating Understanding a New Trend: In Situ Cleaning and Coating Understanding a New Trend: In Situ Cleaning and Coating


Every corrosion, abrasion, or erosion issue can present its own unique set of problems and associated solutions, each bearing its own merit...

6 Ways to Prevent Corrosion Failure Analysis Frustration 6 Ways to Prevent Corrosion Failure Analysis Frustration 6 Ways to Prevent Corrosion Failure Analysis Frustration 6 Ways to Prevent Corrosion Failure Analysis Frustration


This article discusses how to work with a metallurgical lab to increase the likelihood of getting the information needed to determine the...

concrete surface preparation concrete surface preparation concrete surface preparation concrete surface preparation


Concrete may need to be prepared for repairs and overlays, or to clean and/or roughen the surface for the application of a subsequent...

quenching metal steel quenching metal steel quenching metal steel quenching metal steel


The quenching of metals is used in the manufacture of various types of steel. The metallurgical processes involved in quenching can enhance...

3 Essential Types of Material Destructive Tests 3 Essential Types of Material Destructive Tests 3 Essential Types of Material Destructive Tests 3 Essential Types of Material Destructive Tests


Tensile, toughness and fatigue destructive testing provides valuable information for determining the suitability of a material in a...

Elemental Strategies of Coatings Asset Management: Terry Greenfield Q&A Elemental Strategies of Coatings Asset Management: Terry Greenfield Q&A Elemental Strategies of Coatings Asset Management: Terry Greenfield Q&A Elemental Strategies of Coatings Asset Management: Terry Greenfield Q&A


A NACE International instructor and trainer in corrosion assessment, Terry Greenfield has 40 years’ experience in protective coatings...

Practical Techniques for Cathodic Protection Potential Measurement Practical Techniques for Cathodic Protection Potential Measurement Practical Techniques for Cathodic Protection Potential Measurement Practical Techniques for Cathodic Protection Potential Measurement


In order to determine the adequacy of a cathodic protection system applied on a certain structure, its polarized potential has to be...

Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 2) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 2) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 2) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 2)


A decade of independent surface preparation studies show no correlation between higher surface profiles and protective coating adhesion;...

Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 1) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 1) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 1) Myth or Fact: Higher Surface Profile Increases Coating Adhesion (Part 1)


As the corrosion control industry adopts new coating technologies, the debate continues regarding best practices in steel surface...

Effective Home Remedies for Treating Surface Corrosion Effective Home Remedies for Treating Surface Corrosion Effective Home Remedies for Treating Surface Corrosion Effective Home Remedies for Treating Surface Corrosion


Learn some of the numerous DIY home and workshop remedies you can apply to improve matters before having to accept defeat in the name of a...

Ice Pigging: New European Pipe Cleaning Innovation Ice Pigging: New European Pipe Cleaning Innovation Ice Pigging: New European Pipe Cleaning Innovation Ice Pigging: New European Pipe Cleaning Innovation


A water infrastructure corrosion expert reviews a paper by researchers at the University of Bristol on an innovative technique called ice...