Corrosion Prevention
Parent Tag for articles relating to corrosion prevention.
6 Things You Need to Know About Platinized Titanium Anodes
Platinized titanium anodes are preferred in impressed current cathodic protection systems exposed to marine environments due to the low...
Is Surface Preparation for Concrete Repairs a Fad?
Proper attention to surface preparation is essential to achieve a robust bond between repair materials and the existing concrete substrate....
Correcting and Preventing Concrete Corrosion
Corrosion of reinforcing steel in concrete is a worldwide problem that causes a range of economic, aesthetic and utilization issues....
Corrosion Fatigue of Welded Joints on Marine Offshore Structures
When combined, fatigue and corrosion have an exponentially worse effect on the reliability and lifespan on marine offshore structures and...
How to Stop a Ship's Marine Corrosion in 3 Steps
Discover the three-step process to stop corrosion in metal ships: identify marine corrosion, understand the cause and eliminate the cause.
Industry Experts Discuss Subsea Pipeline Corrosion Management
In this exclusive interview, three oil & gas industry corrosion experts discuss some of the key challenges in protecting subsea assets from...
Salt Limits to Prevent Premature Coating Failures
The presence of non-visible residual surface salts and their impact on life cycle coating performance is well documented, yet no widespread...
Flexible Coatings for Protection of Marine Structures
Protecting offshore structures from corrosion and abrasion damage is an ongoing and costly challenge for operators. A polyurea coatings...
EIT Corrosion Detection Systems: Are They the Future?
Grouted electrically isolated pre-tensioned tendons provide advantages for prestressed concrete structures such as bridges and flyovers....
Electric Transportation Systems and Stray Current Corrosion
Stray current corrosion from DC transit system is a real threat to a pipeline’s integrity, but it can be detected by measuring the...
Corrosion Knowledge Management Vs. Corrosion Management: An Essential Tool for Assets Integrity Management
A model for material management called Corrosion Knowledge Management (CMK) may be applied by both corrosion experts and non-corrosionists...
Coatings Advances: Nanoparticle Technology and Cold Sprays
Multilayer deposition of nano particles, formation of smart coatings and field trials of cold sprays are the significant developments...
Corrosion Management in Water Treatment: A Look at Water Pipeline Corrosion and Why It's Becoming a Problem
Drinking water travels through metallic pipes. The corrosion rate depends upon dissimilar metals used in pipes and water parameters such as...
IOZ Coating Surface Preparation Is Easier than You Think
From edge treatment to salt removal, the requirements for applying single-coat inorganic zinc silicate (IOZ) coatings are not difficult for...
Why Pigging Out Is A-OK When It Comes to Cleaning Pipelines
This article examines pipeline operational pigging for internal corrosion prevention, including requirements, pig types, pig selection,...
Pitting Corrosion Prevention: How to Protect and Monitor Metallic Surfaces
Pitting corrosion is a dangerous form of deterioration. It can be prevented by choosing metals with appropriate pitting corrosion...
The Characteristics of and Applications for Fluoropolymer Coatings
Fluoropolymer coatings have a combination of desirable properties, including weatherability and corrosion barrier protection. They have...
Multi-Technique Pipeline Corrosion Monitoring
Individual corrosion monitoring techniques can be misleading and indicate no corrosion or only one type of corrosion. Here, we take a look...
Solving Multilayer Coating Delamination Issues During Pipeline Installation
During the installation of pipelines with multilayer coating systems, it is not uncommon for delamination to occur in the cutback area of...