Filiform corrosion on painted aluminum. Filiform corrosion on painted aluminum. Filiform corrosion on painted aluminum. Filiform corrosion on painted aluminum.


Filiform corrosion is a form of corrosion that occurs under thin coatings, especially on aluminum and magnesium substrates. It can be...

Pipeline with corrosion under insulation CUI Pipeline with corrosion under insulation CUI Pipeline with corrosion under insulation CUI Pipeline with corrosion under insulation CUI


Chloride, galvanic, acidic or alkaline corrosion can cause corrosion under insulation (CUI), but there are ways to prevent the problem.

Old iron trailer with rust Old iron trailer with rust Old iron trailer with rust Old iron trailer with rust


The corrosion or rusting of iron creates a reddish-brown hydrated iron oxide. Understanding how iron…

Paper mill with stainless steel process vessels. Paper mill with stainless steel process vessels. Paper mill with stainless steel process vessels. Paper mill with stainless steel process vessels.


Austenitic stainless steels are susceptible to caustic cracking. We discuss environments where this is common, how to identify it, and how...

Oil refinery with stainless steel process equipment and pipelines. Oil refinery with stainless steel process equipment and pipelines. Oil refinery with stainless steel process equipment and pipelines. Oil refinery with stainless steel process equipment and pipelines.


Polythionic acid stress corrosion cracking of austenitic stainless steel can be prevented by an appropriate soda ash neutralization...

Soluble Salts and Coating Performance Soluble Salts and Coating Performance Soluble Salts and Coating Performance Soluble Salts and Coating Performance


Due to the potential for soluble salts to reduce coating performance, testing the substrate for the presence of these salts should be...

Pipes in seawater. Pipes in seawater. Pipes in seawater. Pipes in seawater.


The chemical reactions responsible for the corrosion of pipes in seawater environments are predominantly electrochemical in nature, so...

Offshore oil rig Offshore oil rig Offshore oil rig Offshore oil rig


Zinc is widely used in the oil & gas industry, but its safety is being called into question by regulators and the industry, especially for...

The Anatomy of a Coating Failure The Anatomy of a Coating Failure The Anatomy of a Coating Failure The Anatomy of a Coating Failure


Rarely does a coating fail because of only one contributing factor. Rather, it is usually two or more factors working in conjunction that...

Ultrasonic Crack Inspection: How to Avoid Pipeline Failures Ultrasonic Crack Inspection: How to Avoid Pipeline Failures Ultrasonic Crack Inspection: How to Avoid Pipeline Failures Ultrasonic Crack Inspection: How to Avoid Pipeline Failures


Ultrasonic technology uses sound waves to detect cracks and other pipeline defects. The early identification of these cracks is essential...

View of river water in Flint, Michigan View of river water in Flint, Michigan View of river water in Flint, Michigan View of river water in Flint, Michigan


Brown discolored water began appearing in a city’s drinking water after a change to the water supply. Further investigations revealed the...

Salt Limits to Prevent Premature Coating Failures Salt Limits to Prevent Premature Coating Failures Salt Limits to Prevent Premature Coating Failures Salt Limits to Prevent Premature Coating Failures


The presence of non-visible residual surface salts and their impact on life cycle coating performance is well documented, yet no widespread...

Engineering Ships for Better Coating Performance Engineering Ships for Better Coating Performance Engineering Ships for Better Coating Performance Engineering Ships for Better Coating Performance


When examining why marine coatings fail, the industry commonly assumes the cause lies in substandard surface preparation or paint...

Pitting Corrosion Prevention: How to Protect and Monitor Metallic Surfaces Pitting Corrosion Prevention: How to Protect and Monitor Metallic Surfaces Pitting Corrosion Prevention: How to Protect and Monitor Metallic Surfaces Pitting Corrosion Prevention: How to Protect and Monitor Metallic Surfaces


Pitting corrosion is a dangerous form of deterioration. It can be prevented by choosing metals with appropriate pitting corrosion...

INFOGRAPHIC: The Flixborough Disaster INFOGRAPHIC: The Flixborough Disaster INFOGRAPHIC: The Flixborough Disaster INFOGRAPHIC: The Flixborough Disaster


In 1974, a chemical plant in Flixborough, England exploded, resulting in multiple deaths and millions of dollars in damages. This disaster...

A Monstrous Coating Failure and How We Fixed It A Monstrous Coating Failure and How We Fixed It A Monstrous Coating Failure and How We Fixed It A Monstrous Coating Failure and How We Fixed It


A renowned corrosion expert, author and past president of NACE International recounts one of the most challenging coating failures he...

Understanding Pitting Corrosion to Prevent Catastrophic Failures Understanding Pitting Corrosion to Prevent Catastrophic Failures Understanding Pitting Corrosion to Prevent Catastrophic Failures Understanding Pitting Corrosion to Prevent Catastrophic Failures


Pitting corrosion, although relatively small in size, can result in catastrophic failures in a variety of structures. Its unpredictability...

INFOGRAPHIC: The El Paso Natural Gas Company Pipeline Explosion INFOGRAPHIC: The El Paso Natural Gas Company Pipeline Explosion INFOGRAPHIC: The El Paso Natural Gas Company Pipeline Explosion INFOGRAPHIC: The El Paso Natural Gas Company Pipeline Explosion


In August of 2000, the 30-inch diameter El Paso Natural Gas Company pipeline exploded in New Mexico resulting in 12 deaths and millions of...

Increased Rates of Copper Corrosion in the Zone of Aeration Explained Increased Rates of Copper Corrosion in the Zone of Aeration Explained Increased Rates of Copper Corrosion in the Zone of Aeration Explained Increased Rates of Copper Corrosion in the Zone of Aeration Explained


Variation in environmental conditions tends to create conditions ideal for the formation of differential aeration cells in the zone of...