Accelerated Testing of Industrial Protective Coatings

Description


This technology update describes laboratory experiments, applications, and typical uses for accelerated testing of industrial protective coatings. This document describes only laboratory experiments. In an industrial setting protective coatings are used for a variety of reasons. Service environments for protective coatings may range from a mild atmospheric exposure condition to a severe chemical or immersion setting.