SSPC-TU 3

Specifications


Process:  Application
Substrate:  Carbon Steel, Stainless Steel, Aluminum, Misc. Alloys

Summary


Factors and Risks Associated with Overcoating

Description


This technology update discusses the risks associated with the maintenance painting practice known as overcoating. Factors affecting overcoating application, service and costs are discussed. This document is intended to serve as a resource for facility owners and others charged with developing and implementing maintenance painting programs. Overcoating is one of several maintenance painting options. This document is not intended to provide a detailed description or comparison of the relative merit and cost considerations of overcoating versus other maintenance painting options. For a more complete and detailed discussion of maintenance painting practices, the reader should refer to SSPC-PA Guide 5, Guide to Maintenance Painting Programs.