SSPC-TR 3/NACE 6A192

Specifications


Asset:  Bridge, Offshore Structure, Onshore Structure, Pressure Vessel
Industry:  Oil and Gas, Energy Generation and Distribution, Water and Wastewater, Transportation Infrastructure, Maritime, Pulp and Paper
Process:  Application

Summary


Dehumidification and Temperature Control

Description


This joint technical report presents current information about why and how dehumidification and temperature control are being used to achieve higher-quality coating/lining projects. It discusses methods of dehumidification, sizing equipment, the impact of contaminants and relative humidity, the uses of dehumidification and temperature control equipment, and inspection instrumentation. An appendix provides information about the relative humidities at which different contaminants can bring moisture to the surface.