Summary


Thermal Pre-Cleaning

Description


This joint technical report addresses the use of thermal pre-cleaning for tanks, vessels, rail tank cars and hopper cars, and process equipment when preparing surfaces for the application of high-performance or high-bake coating and lining systems.