SSPC-SP WJ-1/NACE WJ-1

Share this:

By: NACE/SSPC


SSPC-SP WJ-1/NACE WJ-1

Specifications


Asset:  Bridge, Offshore Structure, Onshore Structure, Pipeline
Environmental Characteristic:  Brackish Water, Fresh Water, High Humidity, Low Humidity
Industry:  Oil and Gas, Pipelines and Underground Systems, Energy Generation and Distribution, Water and Wastewater, Transportation Infrastructure, Maritime, Pulp and Paper, Misc. Corrosion
Process:  Surface Preparation
Substrate:  Copper, Brass, Carbon Steel, Stainless Steel, Aluminum, Misc. Alloys

Summary


Waterjet Cleaning of Metals, Clean to Bare Substrate

Description


SP WJ-1 contains requirements for cleaning metals to bare substrate using waterjet cleaning, including the required end condition of the surface and procedures and materials necessary to achieve the end condition.