SSPC-PS Guide 8.00


SSPC-PS Guide 8.00

Specifications


Process:  Application
Substrate:  Carbon Steel

Summary


Guide to Topcoating Zinc-Rich Primers

Description


This guide covers the selection and application (including surface preparation) of topcoats to surfaces coated with a zinc-rich primer. Both organic and inorganic zinc-rich primers are included.