SSPC-Paint 39

Share this:

SSPC-Paint 39

Specifications


Asset:  Bridge, Offshore Structure, Onshore Structure, Pipeline
Environmental Characteristic:  Below Freezing Point, High Humidity, Low Humidity
Industry:  Oil and Gas, Pipelines and Underground Systems, Energy Generation and Distribution, Water and Wastewater, Transportation Infrastructure, Maritime, Pulp and Paper, Misc. Corrosion
Process:  Application
Substrate:  Carbon Steel

Summary


Two-Component Aliphatic Polyurea Topcoat Fast or Moderate Drying, Performance-Based

Description


This specification contains performance requirements for a two-component, weatherable polyurea topcoat. The coating may be fast or moderately fast drying. Coatings meeting the requirements of this specification are generally suitable for exposures in Environmental Zones 1A (interior, normally dry), 1B (exterior, normally dry), 2A (frequently wet by fresh water, excluding immersion), and 2B (frequently wet by salt water, excluding immersion). Resistance of polyurea topcoats in Environmental Zones 3B (chemical exposure, neutral) and 3C (chemical exposure, alkaline) can vary based upon formulation. The coating manufacturer should be contacted for specific chemical resistance data if required. The specified coating is intended for application by single-component airless spray, electrostatic spray, or plural-component equipment, depending upon its formulation. This coating is intended for use as a topcoat over suitably primed ferrous metal and cementitious substrates.