SSPC-Paint 24

Share this:

SSPC-Paint 24

Specifications


Asset:  Onshore Structure
Environmental Characteristic:  Low Humidity
Industry:  Maritime, Misc. Corrosion
Process:  Application
Substrate:  Carbon Steel

Summary


Latex Semigloss Exterior Topcoat

Description


This specification covers an air drying, ready-mixed, water-borne semigloss latex paint for use on metal surfaces primed with a primer conforming to SSPC-Paint 23, Latex Primer for Steel Surfaces. It is intended for use as a topcoat of a water-borne coating system consisting of two coats of primer and one or two coats of this water-borne topcoat. \r\nThis paint is suitable for exposures in Environmental Zones 1A (interior, normally dry) and 1B (exterior, normally dry), and is intended for brush, spray, or roller application over properly primed steel surfaces and is to be applied in accordance with SSPC-PA 1, Shop, Field, and Maintenance Painting of Steel. It is not recommended to expose steel to the weather with less than two coats of waterborne coating; therefore, intermediate and topcoats should be applied as soon as possible.