SSPC-Paint 15

Share this:

SSPC-Paint 15

Specifications


Asset:  Onshore Structure
Environmental Characteristic:  High Humidity, Low Humidity
Industry:  Transportation Infrastructure, Maritime
Process:  Application
Substrate:  Carbon Steel

Summary


Steel Joist Shop Primer/Metal Building Primer

Description


This specification covers a one coat shop-applied primer for open web and long span steel joist and joist girders and for cold formed steel framing, and primary and secondary structural framing for metal buildings. This coating is intended to provide temporary protection to the steel joist during delivery, storage on site, and erection in an atmosphere comparable with SSPC Environmental Zone 1, normally dry. This coating is intended to be used as a holding primer that may or may not be removed before or after erection or assembly in the field.\r\n\r\n\r\n\r\nThe specification does not address the formulation of the coating but covers the physical and performance characteristics of the coating.