SSPC-PA Guide 10


SSPC-PA Guide 10

Specifications


Asset:  Bridge, Offshore Structure, Onshore Structure, Pipeline, Pressure Vessel
Environmental Characteristic:  Below Freezing Point, Below Ground, High Heat, High Humidity, Low Humidity, Solvent
Industry:  Oil and Gas, Pipelines and Underground Systems, Energy Generation and Distribution, Water and Wastewater, Transportation Infrastructure, Maritime, Pulp and Paper, Misc. Corrosion
Process:  Application
Substrate:  Copper, Concrete, Brass, Polymers, Laminates, Carbon Steel, Stainless Steel, Aluminum, Misc. Alloys

Summary


Guide to Safety and Health Requirements for Industrial Painting Projects

Description


This guide replaces PA Guide 3. This Guide is intended for facility owners and project specifiers who have a mandate to incorporate appropriate requirements for safety and health program submittals and associated acceptance criteria in contract documents. It also alerts contractors to their responsibilities to protect workers as required by the US. Occupational Safety and Health Administration (OSHA). It also provides examples of contract language that can be incorporated into project specifications.