Guide for Atmospheric Testing of Coatings in the Field

Description


This guide covers the procedures for planning, performing, and documenting field evaluations of atmospheric testing of coatings applied to steel panels or steel structures. It is intended for coating systems applied to new or previously coated structures. It is intended for use by coatings specifiers, end users, manufacturers, formulators, and test laboratories.