Summary


Standard Specification for Zinc and Epoxy Dual-Coated Steel Reinforcing Bars

Description


Abstract:

This specification covers deformed and plain steel reinforcing bars with a dual coating of zinc alloy and an epoxy coating. The zinc alloy layer shall be applied by the thermal spray coating method followed by an epoxy coating, which shall be applied by the electrostatic spray method. The zinc coating shall conform to the required chemical composition for aluminum, cadmium, copper, iron, lead, tin, antimony, silver, bismuth, arsenic, nickel, magnesium, titanium, and zinc. The coated steel reinforcing bars shall conform to bend test requirements and to physical properties such as coating thickness, coating continuity, epoxy coating flexibility, and coating adhesion.1.1 This specification covers deformed and plain steel reinforcing bars with a dual coating of zinc alloy and an epoxy coating. The zinc-alloy layer is applied by the thermal spray coating method (metallizing) followed by an epoxy coating applied by the electrostatic spray method. The coating applicator is identified throughout this specification as the manufacturer.1.2 Requirements of the zinc coating are contained in Table 1.1.3 Requirements for fusion-bonded powder coatings are contained in Annex A1.1.4 Guidelines for construction practices at the job-site are presented in Appendix X1.1.5 This specification is applicable for orders in either inch-pound or SI units.1.6 The values stated in either inch-pound units or SI units are to be regarded as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other, except as specifically noted in Table 2. Combining values from the two systems may result in nonconformance with this specification.1.7