Are there CUI concerns for operating temperatures over 350 degrees F?

Answer
By David Shong | Published: December 18, 2020

Absolutely. Corrosion under insulation (CUI) can be a serious issue for pipes and process equipment covered with thermal insulation. The corrosion range has kind of been established from 100 to 350°F (38 to 177°C) for mild steel, and 350°F is really kind of the upper limit where liquid water can exist before it vaporizes into its gaseous state.

I definitely would not say that only equipment that operates in between that temperature range is subject to CUI. Every piece of equipment in an industrial facility, in my opinion, is subject to CUI because of the high temperature ranges that are often cyclical, which will drop down into the CUI range. And then, also, during maintenance and outages you will see that equipment brought down out of service, and you can see significant amounts of time where it's in that CUI danger range. (Related reading: Third Party Long-Term Testing: CUI & Thermal Results.)

So, definitely, we want to help people understand what that bandwidth is really. Don't think that if you don’t have something operating in that operating condition, then you won't have to worry. CUI can occur at any operating temperature range because of those cyclical and outage conditions.

Figure 1. Pipes covered with thermal insulation.

Figure 1. Pipes covered with thermal insulation. (Source: Kyryl Gorlov/Dreamstime.com)

Advertisement

Share this

  • Facebook
  • LinkedIn
  • Twitter

Written by David Shong

David Shong

David Shong has spent his entire career in the construction materials industry and developed an early passion for insulation. He has worked in the industrial insulation field since 2014.

More Q&As from our experts

Term of the Day

Calcium Silicate

Calcium silicate is a chemical compound composed of calcium and silica with the chemical formula Ca2SiO4 that is naturally…
Read Full Term

Don't miss the latest corrosion content from Corrosionpedia!

Subscribe to our newsletter to get expert advice and top insights on corrosion science, mitigation and prevention. We create world-leading educational content about corrosion and how to preserve the integrity of the world’s infrastructure and assets.

Resources
Go back to top