Orange Peel

Last updated: July 19, 2024

What Does Orange Peel Mean?

Orange peel is a term used to describe a now defective layer of coating applied to a metallic surface to prevent corrosion. The defective coating raises up and curls after a long period since application, and is shaped similarly to the peel of an orange fruit.


Free Coating Failures and Defects Guide – Sponsored by Fitz’s Atlas 2

Coating Failures and Defects Guide
Click here to download your free guide!


Advertisement

Corrosionpedia Explains Orange Peel

An orange peel is usually formed after a significant fallow period of no regular corrosion preventive measures. Implementation of proper corrosion prevention care, as well as regular maintenance, can prevent the orange peel occurrence.

Advertisement

Share This Term

  • Facebook
  • LinkedIn
  • Twitter

Related Reading

Trending Articles

Go back to top

Stay Ahead of the Corrosion Curve

Get expert insights, industry news, and practical tips delivered straight to your inbox. Join our community of corrosion professionals.