RPR Technologies has developed a method of removing all types of coatings by using an induction dis bonding machine known as the RPR. The RPR works by the principle of induction. Heat is generated in the steel substrate and the bond is broken between the coating and the steel. The coating is then removed entirely without disintegrating and completely free from contaminating agents, i.e. blast media. This makes containment and disposal easier and cheaper. Paint and other coatings such as hard and soft rubber, 3LPE, PFP, GRP/GRE are easily removed with the RPR. The RPR is not only the world’s fastest method for removing paint and coatings from steel surfaces, it also provides a safe and clean working environment, an obvious requirement for all of us.